80 lb quikrete crack resistant concrete mix or 80 lb quikrete concrete mix or 80 lb quikrete 5000 concrete mix.
Quikrete high strength concrete mix.
This concrete mix is designed for applications requiring high early strength and rapid strength gains.
Achieves 5000 psi after 28 days.
Properly graded sand and gravel blended with portland cement for use as in general concrete applications.
1229 86 shotcrete ms ar fiberglass reinforced no.
For any concrete use requiring high early strength and rapid strength gains where superior workability is desired.
1229 83 shotcrete ms steel fiber reinforced no.
Quikrete 5000 concrete mix no.
Quikrete concrete mix exceeds the compressive strength requirements of astm c387 as shown in table 1.
Made from a special blend of sand coarse aggregate and cementitious materials this concrete mix can be used for new construction or repairs where concrete thickness exceeds 2 in.
5000 high early strength concrete mix consists of a commercial grade blend of portland cement sand gravel.
High strength concrete mix is sakrete 80 lb.
1007 is a commercial grade blend of stone or gravel sand and cement specially designed for higher early strength.
High strength concrete mix is a high quality mix designed to provide outstanding strength and durability.
Quikrete 5000 high early strength concrete mix no.
Use for any general concrete work.
More product details close.
1228 21 shotcrete ms no.
03 37 13 shotcrete.
1229 80 shotcrete ms poly fibers reinforced no.
5000 high early strength concrete mix has a walk on time of 10 12 hours.
This concrete mix is designed for applications requiring high early strength and rapid strength gains.
Ideal for cold weather application.
Quikrete concrete mix no.
The more water that is added to the mix the weaker it becomes.
It is a perfect mix for both the diy er and contractor that are looking for a concrete with rapid strength gain.
1007 data sheet sds document.
1101 is the original 4000 psi average compressive strength blend of portland cement sand and gravel or stone.
Table 1 typical compressive strength1 compressive strength astm c39 age typical values 7 days 2500 psi 17 2 mpa 28 days 4000 psi 27 6 mpa slump range 2 3 51 76 mm.